Ptfe Pfa Wafer Lined Check Valve
- Place of Origin:
- Wenzhou,China
- Packing:
- Suitable Packing for Sea/Air Transport
- Connection:
- Wafer Type
- Pressure:
- PN10,PN16,150LBS
- Temperature:
- PTFE:-29℃ ~180℃, PFA:-29℃~200℃, FEP:-29℃~150℃
A lined check valve stops process inversion inside tight pipe layouts when forward fluid pressure pushes an encapsulated disc away from its annular seating perimeter. Decreasing forward line pressure allows process backpressure to force the disc against the resilient seating face instantaneously, delivering bubble-tight isolation against aggressive chemical reagents.
Fluoroplastic Isostatic Compression and Vacuum Retention Anchoring
Processing piping handling hot concentrated sulfuric acid or halogen mixtures relies on a ptfe lined check valve engineered to withstand aggressive chemical oxidation up to 180°C. Sintered polytetrafluoroethylene resin creates dense, non-porous barriers that prevent chemical seepage into outer metallic housings.
Machining precision dovetail locking channels throughout ductile iron body interiors locks the protective polymer envelope mechanically. This mechanical retention stops lining collapse during pump shutdown cycles, siphon drainage, or full vacuum conditions.
Industrial Inter-Flange Flow Control Selection Parameters
| Internal Closure Geometry | Pipeline Spool Mounting | Tightness Standard | Target Media Application |
|---|---|---|---|
| Hinged Encapsulated Flap | Wafer Inter-Flange Mount | API 598 Bubble-Tight | Hot inorganic acid streams |
| Guided Axial Piston | Flanged Horizontal Line | ISO 5208 Rate A Shutoff | Clean chemical effluents |
| Free Floating Core | Flanged Vertical Spool | MSS SP-72 Class VI Tightness | Entrained particulate slurries |
Matching closure travel distance with line velocity limits flow resistance and preserves sealing interfaces.
Hydrodynamic Disc Rotation and Low Pressure Sealing Mechanics
Chemical facilities operating pfa lined ball check valves frequently observe heavy pressure loss inside horizontal headers because spherical bodies consume substantial flow cross-sections. Spheres also wobble under turbulent discharge, accelerating perimeter erosion and delaying closure response.
The wafer swing structure employs an encapsulated disc pivoting smoothly inside an internal hinge axis isolated from corrosive media. This constrained motion path stabilizes fluid vectors, suppresses disc fluttering, and eliminates binding during rapid pressure fluctuations.
Companion Flange Centering and Uniform Torque Fastening
Demanding operating environments reach extended durability through a pfa lined check valve when process parameters exceed standard thermal limits, whereas virgin PTFE ensures economical resistance at moderate temperatures. Uniform liner wall thickness across intricate internal contours stops acidic fluids from contacting pressure-retaining metal shells.
Field crews tighten companion flange studs with calibrated torque wrenches using sequential cross-pattern passes. Balanced bolt compression prevents uneven mechanical loading across raised sealing faces, stopping localized cold flow creep.
Providing five straight pipe diameters upstream eliminates boundary layer swirl, preserving internal polymer contours throughout continuous chemical processing operations.
Product Parameter
Materials of Main Parts
| No. | Part Name | Material List | |||||
| 1 | Body/Bonnet | HT250 | WCB | CF8 | CF8M | CF3 | CF3M |
| 2 | Disc/Stem | 25 1Cr18Ni19/CF8 00Cr17Ni14Mo2/CF3M | |||||
| 3 | Lining/Seat | PCTFE(F3) FEP(F46) PTFE(F4) PFA PO | |||||
| 4 | Bolt | 35 | 35 | 0Cr18Ni9 | 0Cr18Ni9 | 0Cr18Ni9 | 0Cr18Ni9 |
| 5 | Nut | 45 | 45 | 0Cr18Ni9 | 0Cr18Ni9 | 0Cr18Ni9 | 0Cr18Ni9 |
Technical Specification
| Design & Manufacture Standard | GB/T 12236 | API 6D | ||
| Face-to-face Dimension Standard | GB/T 12221 | ASME B16.10 | ||
| Flange Standard | HG/T 20592 | ASME B16.5 | ||
| Inspection and Test Standard | GB/T 13927 | API 598 | ||
| Nominal Pressure | 1.0MPa | 1.6Mpa | 150LB | |
| Test Pressure | Shell Test | 1.5MPa | 1.5MPa | 1.5MPa |
| High Pressure Sealing | 1.1MPa | 1.1MPa | 1.1MPa | |
| Low Pressure Sealing | 0.6MPa | 0.6MPa | 0.6MPa | |
| Temperature Range | PFA:-29℃~200℃ PTFE:-29℃~180℃ FEP:-29℃~150℃ | |||
| Applicable Medium | Strong corrosive medium i.e.hydrochloric acid,Nitric acid,Hydrofluoric acid,Liquid chlorine,Sulfuric acid and Aqua regia etc. | |||
| Note:Test standard refers to general valve standard,high pressure should be customized for processing. | ||||